Nickel 200 Superalloys

Nickel 200

NICKEL 201, Nickel 200,

Nickel 200 Datasheet

Nickel 200 Superalloys: ASTM B160 Chemical composition

C Si Mn S Ni Cu Fe Mg Ti Co
≤0.15 ≤0.35 ≤0.35 ≤0.01 Bal- ≥ ≤0.25 ≤0.40 ≤0.20 ≤0.10 ≤2.00

Nickel 200 Superalloys: ASTM B160 specification

  • ASTM B160 -
  • ASTM B162 -
  • BS 3075 NA11 -
  • BS 3076 NA11 -

Nickel 200 Superalloys - mechanical properties

Heat treatment Min Max Similar Note
Heat treatment Min Max Similar Note
Heat treatment Min Max Similar Note
Heat treatment Min Max Similar Note
Heat treatment Min Max Similar Note
Heat treatment Type Min Max Similar Note
  • Electronic components.
  • Electrical components.
  • Lead in wires for heating elements.
  • Battery connections/terminals.
  • Chemical processing.
  • Aerospace components..
  • Food processing.
  • Synthetic fibre processing.
Density8.89 g/cm³0.321 lb/in³
Melting Point1446°C2635°F
Coefficient of Expansion13.3 μm/m °C (20 – 100°C)7.4 x 10-6 in/in °F (70 – 212°F)
Modulus of Rigidity81 kN/mm²11748 ksi
Modulus of Elasticity204 kN/mm²29588 ksi
Electrical Resistivity
9.6 μΩ • cm58 ohm • circ mil/ft
Thermal Conductivity
70.2 W/m • °C487 btu • in/ft2 • h • °F
> Properties
ConditionApprox. tensile strengthApprox. operating temperature
N/mm²ksi
Annealed400 – 50058 – 73Tensile strength and elongation drop significantly at temperatures above
315°C (600°F). Service temperature is dependent on environment, load and size range.